性能项目 | 测试条件 | 测试方法 | 数值/描述 | 单位 | |
机械性能 | 拉伸强度(引张强度) | ASTM D638/ISO 527 | 450(6,380) | kg/cm⊃2;(MPa)[Lb/in2] | |
断裂伸长率 | ASTM D638/ISO 527 | -- | % | ||
拉伸模量 | ASTM D638/ISO 527 | -- | kg/cm⊃2;(MPa)[Lb/in2] | ||
拉伸屈服伸长率(延伸率) | ASTM D638/ISO 527 | 15 | % | ||
拉伸断裂伸长率(延伸率) | ASTM D638/ISO 527 | -- | % | ||
弯曲模量(弯曲弹性率) | ASTM D790/ISO 178 | 23000(32000) | kg/cm⊃2;(MPa)[Lb/in2] | ||
弯曲强度 | ASTM D790/ISO 178 | 680(9,650) | kg/cm⊃2;(MPa)[Lb/in2] | ||
洛氏硬度 | ASTM D785 | R-115 | |||
IZOD 缺口冲击强度 | 1/4' 23℃ | ASTM D256/ISO 179 | -- | kg·cm/cm(J/M)ft·lb/in | |
1/4' -30℃ | ASTM D256/ISO 179 | 14(2.6 | kg·cm/cm(J/M)ft·lb/in | ||
1/8' 23℃ | ASTM D256/ISO 179 | -- | kg·cm/cm(J/M)ft·lb/in | ||
1/8' -30℃ | ASTM D256/ISO 179 | 17(3.2) | kg·cm/cm(J/M)ft·lb/in | ||
Charpy冲击强度 | 23℃ (缺口) | ASTM D256/ISO 179 | -- | kg·cm/cm(J/M)ft·lb/in | |
-30℃(缺口) | ASTM D256/ISO 179 | -- | kg·cm/cm(J/M)ft·lb/in | ||
23℃(无缺口) | ASTM D256/ISO 179 | -- | kg·cm/cm(J/M)ft·lb/in | ||
-30℃(无缺口) | ASTM D256/ISO 179 | -- | kg·cm/cm(J/M)ft·lb/in | ||
物性性能 | 比重(密度) | ASTM D792/ISO 1183 | 1.06 | ||
成型收缩率 | ASTM D955 | -- | % | ||
熔融指数(流动系数) | 200℃/5kg | ASTM D1238/ISO 1133 | -- | g/10min | |
220℃/10kg | ASTM D1238/ISO 1133 | 5.5 | g/10min | ||
吸水率 23℃/24H | ASTM D570/ISO 62 | -- | % | ||
热性能 | 热变形温度 | 退火 | ASTM D648/ISO 75 | 115(239) | ℃(℉) |
未退火 | ASTM D648/ISO 75 | 105(221) | ℃(℉) | ||
维卡软化点 | ASTM D1525/ISO R306 | 125(257) | ℃(℉) | ||
熔点 | - | -- | ℃(℉) | ||
燃烧性(率) | UL94 | 1.6mmHB | |||
线性膨胀系数 | ASTM D696/ISO 11359 | -- | mm/mm.℃ | ||
加工条件 | 干燥条件 | 90~105°C下烘料约3小时 | |||
加工温度 | 射嘴 | 220~250°C | ℃ | ||
料筒前段 | 230~250 °C | ℃ | |||
料筒中段 | 230~250 ℃ | ℃ | |||
料筒后段 | 220~240 ℃ | ℃ | |||
熔体温度 | -- | ℃ | |||
模具温度 | 30~70°C | ℃ | |||
压力 | 注塑压力 | 50~70kg/cm⊃2; | Mpa | ||
保压压力 | 40~60kg/cm⊃2; | Mpa | |||
背压 | 5~15kg/cm⊃2; | Mpa | |||
螺杆转速 | -- | rpm | |||
其他 | 备注 | 在射出周期中勿将热融胶长期停留在加热管中 | |||
颜色 | -- | ||||
特性 | 超耐热性、中冲击强度 | ||||
用途 | 发热家电外壳 / 乾发吹风筒 / 熨斗外壳 / 暖风机 / 汽车零配件如仪表板 / 水箱护罩等 |